Preparation of leady oxide for lead–acid battery by ...
Leady oxide oxidized at 400°C for 1 h and pulverized by ball milling for 1 h after preparation of sponge lead in wt.% HCl solution is shown in Fig. general, Bartonpot leady oxide has a spherical shape and ballmill oxide has a nonuniform platelike shape.